Powder coating really looks good on the Shopsmith equipment. I found I could use the powder coating oven (converted stove) to bake the Rustoleum hammered paint at 200 deg for about 2 hours really harden the paint so I could use the part that day. Quicker and easlier than powder coating. Other brands of paint did burn so would recommend doing a test piece first.