finish recomendation ?

This is a forum for intermediate to advanced woodworkers. Show off your projects or share your ideas.

Moderator: admin

jonesuh
Gold Member
Posts: 67
Joined: Thu Jul 02, 2009 12:48 pm
Location: Houston TX

finish recomendation ?

Post by jonesuh »

I'm building a book case for my son---have some very nice quarter sawn white oak---what is the best way to highlight the natural wood---i would like a "natural wood" look and ---I have heard I should use some sort of 'light" stain
recommendations?
ERLover
Platinum Member
Posts: 3914
Joined: Mon Aug 31, 2015 10:19 pm
Location: Greenie and Goldie Country not to metion the WI Badgers!

Re: finish recomendation ?

Post by ERLover »

You use a 50/50 mix of BLO and MS, wiped on then wipe off excess, or MinWax natural stain which is about the same thing.
KNOWLEDGE AND EXPERIENCE EQUALS WISDOM. Albert Einstein
The Greatness officially starts :D :D :D :D :D :D
Greenie, Grayling, SS stand alone BS and BS SPT, jointer and belt sander, 3 Ers with Speed Changers. I think those 3 cover my ER needs, and space for them. :)
User avatar
videobear
Gold Member
Posts: 180
Joined: Tue Aug 21, 2012 12:24 pm
Location: northern VA

Re: finish recomendation ?

Post by videobear »

I used a light oak stain on my kids' desks and bookcases, followed by several coats of wipe-on polyurethane varnish, with a hand sanding with a fine steel wool pad between coats. Looked good, and withstood everything they could throw at it during their growing up years.
User avatar
BuckeyeDennis
Platinum Member
Posts: 3802
Joined: Tue Jul 24, 2012 10:03 pm
Location: Central Ohio

Re: finish recomendation ?

Post by BuckeyeDennis »

+1 on the wipe-on poly. Easy, durable, and looks nice for most projects.

But more importantly, test your candidate finish(es) on a piece of matching wood scrap, before applying to your project!
mediadaddy
Silver Member
Posts: 13
Joined: Wed Mar 16, 2011 9:43 pm
Location: Parachute,CO

Re: finish recomendation ?

Post by mediadaddy »

I'll add, a coat of shellac or two first- retards splotchiness that might occur.
Hobbyman2
Platinum Member
Posts: 2660
Joined: Wed Feb 01, 2017 12:52 am
Location: Ohio

Re: finish recomendation ?

Post by Hobbyman2 »

Depends if you want a shine that will last for years or a flat surface that will scuff . On book cases or a desk I would suggest considering using tung oil and different grades of wet sand paper like they use in auto body work ,,,,starting from around 220 grit and ending around 1000 grit , the system involves some work but will last for a long time,,,, dip the sand paper in a bowl of tung oil or pour some out on the wood and wet sand it in , let it dry for a few hrs and then do it again with the next higher grade paper ,,,,, after a couple coats let it dry over night ,then keep on going like this until you get to 1000 or higher grit ,I normally do this using 4 grits and it takes 2 days to finish ,,, you will be amazed at the grain quality you will get and after a week or two the surface will be very hard ,, the longer it sets the harder it will get.

If you want a flat surface then the above answers are spot on.

You can also use spray on lacquer in rattle cans to bring out the grain,,it usually takes several coats .
Hobbyman2 Favorite Quote: "If a man does his best, what else is there?"
- General George S. Patton (1885-1945)
User avatar
thunderbirdbat
Platinum Member
Posts: 837
Joined: Sat Aug 08, 2015 11:23 am
Location: Marion, Iowa

Re: finish recomendation ?

Post by thunderbirdbat »

Hobbyman2 wrote:Depends if you want a shine that will last for years or a flat surface that will scuff . On book cases or a desk I would suggest considering using tung oil and different grades of wet sand paper like they use in auto body work ,,,,starting from around 220 grit and ending around 1000 grit , the system involves some work but will last for a long time,,,, dip the sand paper in a bowl of tung oil or pour some out on the wood and wet sand it in , let it dry for a few hrs and then do it again with the next higher grade paper ,,,,, after a couple coats let it dry over night ,then keep on going like this until you get to 1000 or higher grit ,I normally do this using 4 grits and it takes 2 days to finish ,,, you will be amazed at the grain quality you will get and after a week or two the surface will be very hard ,, the longer it sets the harder it will get.

If you want a flat surface then the above answers are spot on.

You can also use spray on lacquer in rattle cans to bring out the grain,,it usually takes several coats .
Would Teak oil work the same? My husband brought me home a can of it the other day but I have never used it before.
Brenda

1998 510 upgraded to a 520, upgraded to power pro with double tilt and lift assist.
1998 bandsaw
2016 beltsander
jointer
overarm pin router
Sazerac81
Gold Member
Posts: 224
Joined: Fri Feb 19, 2016 1:33 am

Re: finish recomendation ?

Post by Sazerac81 »

General Finishes ArmRseal. 3-7 wipe on coats depending on your patience. Lightly sand in between with 400 grit or higher paper. Then follow with a buffing wax like Renaissance Wax or Minwax furniture wax and buff it down. Awesome, long lasting finish and surface.

The GF polyacrylic finishes are also top notch if you want low VOCs and water solubility. It doesn't bring out the grain as much though, but provides a very durable surface and UV stabilization/protection over stains.

Cheers,
John
Hobbyman2
Platinum Member
Posts: 2660
Joined: Wed Feb 01, 2017 12:52 am
Location: Ohio

Re: finish recomendation ?

Post by Hobbyman2 »

thunderbirdbat wrote:
Hobbyman2 wrote:Depends if you want a shine that will last for years or a flat surface that will scuff . On book cases or a desk I would suggest considering using tung oil and different grades of wet sand paper like they use in auto body work ,,,,starting from around 220 grit and ending around 1000 grit , the system involves some work but will last for a long time,,,, dip the sand paper in a bowl of tung oil or pour some out on the wood and wet sand it in , let it dry for a few hrs and then do it again with the next higher grade paper ,,,,, after a couple coats let it dry over night ,then keep on going like this until you get to 1000 or higher grit ,I normally do this using 4 grits and it takes 2 days to finish ,,, you will be amazed at the grain quality you will get and after a week or two the surface will be very hard ,, the longer it sets the harder it will get.

If you want a flat surface then the above answers are spot on.

You can also use spray on lacquer in rattle cans to bring out the grain,,it usually takes several coats .
Would Teak oil work the same? My husband brought me home a can of it the other day but I have never used it before.

===================

I have not used teak oil enough to say one way or another,I know there was a formbys {sp} kit that I believe used it ,,, you can test it if you have a scrap piece of wood , keep in mind no mater what you use will darken the wood a little , I have used tung oil that didn't darken the wood so much ,,,and lin seed oil with good results , .I used this system on the for end I just made , you can see by the results how it brought out the grain.
Hobbyman2 Favorite Quote: "If a man does his best, what else is there?"
- General George S. Patton (1885-1945)
dynabase
Gold Member
Posts: 161
Joined: Sun May 26, 2013 1:06 am
Location: Post Falls, Idaho

Re: finish recomendation ?

Post by dynabase »

Ammonia fumes. It's a traditional "stain" for White Oak. Followed by BLO and wax.

Michael
Post Reply