It appears that a lot of parts (like the strip sander platens) were at one time blued. Does anyone have experience with the process and what it takes to hold corrosion at bay after bluing? Do those of you who do restoration bother to renew the bluing, or just preserve the metal some other way? Is it as hazardous a process as I have been led to believe? Any preferences as to which process/ product?
Thanks
Steel bluing
Moderator: admin
-
dstensland
- Gold Member
- Posts: 42
- Joined: Wed Aug 14, 2013 10:55 pm
- Location: Slaterville Springs, NY
Last year I used some of that Birchwood Casey cold bluing stuff to fix up a Shopsmith riving knife assembly that was inadvertently de-blued while dunked in Evapo-Rust. In the end I was happy with the outcome. The riving knife was well-derusted and almost as good as new. I wasn't doing a showcase restoration but the Birchwood Casey did work better than I had expected.
I also de-blued/re-blued a saw arbor but skipped the waxing. Little bits of surface rust appeared a few months later, so nubobby's wax suggestion is a good one for extra protection.
I also de-blued/re-blued a saw arbor but skipped the waxing. Little bits of surface rust appeared a few months later, so nubobby's wax suggestion is a good one for extra protection.
- "Wild Bad Bob"
- Platinum Member
- Posts: 1065
- Joined: Fri Mar 28, 2014 2:03 pm
- Location: Germantown, Wi
There is 2 types of bluing, hot and cold. The hot is the hazardious one do to stronger/hazardous fumes, in tanks of solution, but does a better job of a bluing coating. Cold bluing is the Birchwood Casey type is a wipe on, and usually takes a few more wipe on coatings to get a finished product.
Measure once, cut as many times as needed to get it right! Bob
56/57 Greenie with jointer, 85 Mark V with band saw, 63 Goldie with jointer, 3 ER 10s, 1951 vintage, Hernia from the Er 10s, Tool Shop SS clone 6" jointer, and 6" belt sander, Delta 10" TS, Buffalo 6" jointer, Craftsman 12" BS, 10" Ryobi planer. Compound Miter, and misc.
56/57 Greenie with jointer, 85 Mark V with band saw, 63 Goldie with jointer, 3 ER 10s, 1951 vintage, Hernia from the Er 10s, Tool Shop SS clone 6" jointer, and 6" belt sander, Delta 10" TS, Buffalo 6" jointer, Craftsman 12" BS, 10" Ryobi planer. Compound Miter, and misc.
- JPG
- Platinum Member
- Posts: 35600
- Joined: Wed Dec 10, 2008 7:42 pm
- Location: Lexington, Ky (TAMECAT territory)
The black oxide is not blueing, but involves heat treating. Think of the 'cold process' as dying.
Quite adequate for intended purpose.
Quite adequate for intended purpose.
╔═══╗
╟JPG ╢
╚═══╝
Goldie(Bought New SN 377425)/4" jointer/6" beltsander/12" planer/stripsander/bandsaw/powerstation /Scroll saw/Jig saw /Craftsman 10" ras/Craftsman 6" thicknessplaner/ Dayton10"tablesaw(restoredfromneighborstrashpile)/ Mark VII restoration in 'progress'/ 10E[/size](SN E3779) restoration in progress, a 510 on the back burner and a growing pile of items to be eventually returned to useful life. - aka Red Grange
╟JPG ╢
╚═══╝
Goldie(Bought New SN 377425)/4" jointer/6" beltsander/12" planer/stripsander/bandsaw/powerstation /Scroll saw/Jig saw /Craftsman 10" ras/Craftsman 6" thicknessplaner/ Dayton10"tablesaw(restoredfromneighborstrashpile)/ Mark VII restoration in 'progress'/ 10E[/size](SN E3779) restoration in progress, a 510 on the back burner and a growing pile of items to be eventually returned to useful life. - aka Red Grange
- dusty
- Platinum Member
- Posts: 21530
- Joined: Wed Nov 22, 2006 6:52 am
- Location: Tucson (Wildcat Country), Arizona
[quote="JPG40504"]The black oxide is not blueing, but involves heat treating. Think of the 'cold process' as dying.
Quite adequate for intended purpose.]
This appears to be a matter of words.
Re: First sentenced in this link.
Quite adequate for intended purpose.]
This appears to be a matter of words.
Re: First sentenced in this link.
"Making Sawdust Safely"
Dusty
Sent from my Dell XPS using Firefox.
Dusty
Sent from my Dell XPS using Firefox.
- "Wild Bad Bob"
- Platinum Member
- Posts: 1065
- Joined: Fri Mar 28, 2014 2:03 pm
- Location: Germantown, Wi
Like rust, bluing is a form of an oxidated protective coating caused by a chemical reaction with the steel/iron. Even though some solutions are heated, it is not the heat in the "bluing process" that causes the color change, it is the chemical reaction causing a colored protective coating.
Now case hardening with "heat" causes a color change in the steel, which can vary based on the steel composition, amount of heat and medium it is quelched in.
Now case hardening with "heat" causes a color change in the steel, which can vary based on the steel composition, amount of heat and medium it is quelched in.
Measure once, cut as many times as needed to get it right! Bob
56/57 Greenie with jointer, 85 Mark V with band saw, 63 Goldie with jointer, 3 ER 10s, 1951 vintage, Hernia from the Er 10s, Tool Shop SS clone 6" jointer, and 6" belt sander, Delta 10" TS, Buffalo 6" jointer, Craftsman 12" BS, 10" Ryobi planer. Compound Miter, and misc.
56/57 Greenie with jointer, 85 Mark V with band saw, 63 Goldie with jointer, 3 ER 10s, 1951 vintage, Hernia from the Er 10s, Tool Shop SS clone 6" jointer, and 6" belt sander, Delta 10" TS, Buffalo 6" jointer, Craftsman 12" BS, 10" Ryobi planer. Compound Miter, and misc.